生物质飞灰未燃尽炭制备活性炭及其超级电容性能研究

Preparation of activated carbon from unburned carbon in biomass fly ash and its supercapacitor performance

  • 摘要: 生物质燃料在锅炉中经过热解和燃烧后,飞灰中含有孔隙丰富的未燃尽炭。但其孔隙率和比表面积无法满足商用超级电容炭的要求,改善材料孔隙结构的活化方法成为未燃尽炭提质改性的关键。本研究通过对筛分粒径 > 0.2 mm的未燃尽炭进行KOH一步活化处理后发现,在浸渍比3.5∶1时活性炭拥有较大的比表面积(1982 m2/g),且在电流密度1 A/g时比电容可达207 F/g。以上结果表明,未燃尽炭基活性炭制备的电极双电层超级电容性能优良,而为生物质飞灰的高附加值利用提供了参考。

     

    Abstract: After the fuel undergoes pyrolysis and combustion in a biomass boiler, the fly ash contains some unburned carbon with abundant pores. However, their low porosities and specific surface areas cannot meet the requirements of the activated carbon for commercial supercapacitors, and the activation method to improve their pore structures is the key to enhance their applicability. After the one-step KOH activation treatment of the unburned carbon with the particle sizes > 0.2 mm, the results showed that the activated carbon has the largest specific area (1982 m2/g) at an impregnation ratio of 3.5∶1, and the specific capacitance reached 207 F/g at the current density of 1 A/g. The above results indicate that unburned carbon-based activated carbon has a good double layer capacitance performance, providing a reference for the high value-added utilization of biomass fly ash.

     

/

返回文章
返回