二甲基硫和乙硫醇在层状K1-2xMxTiNbO5(M=Mn2+、Ni2+)上的吸附与光催化氧化作用

Adsorption and photocatalytic oxidation of dimethyl sulfide and ethyl mercaptan over layered K1-2xMnxTiNbO5 and K1-2xNixTiNbO5

  • 摘要: 采用固相法制备出具有层状结构的KTiNbO5,通过离子交换制备K1-2xMxTiNbO5(M=Mn2+、Ni2+)。采用X射线粉末衍射(XRD)和紫外-可见漫反射光谱技术对样品晶体结构与光谱响应特征进行表征,采用红外光谱方法考察样品对二甲基硫(DMS)和乙硫醇(EM)吸附与光催化氧化行为。结果表明,采用Mn2+和Ni2+对KTiNbO5离子交换后,层板间距增加,对光谱吸收由紫外区移向可见光区,带隙能量由3.35eV相应地移至2.97eV和2.45eV。K1-2xMxTiNbO5对DMS和EM的吸附作用力较弱,不受阳离子影响。K1-2xMnxTiNbO5只在紫外光辐射下呈现催化活性,并将硫醚、硫醇氧化为亚砜、砜和磺酸;而K1-2xNixTiNbO5在可见与紫外光辐射下均具有光催化活性,在可见光辐射下,乙硫醇被氧化至磺酸,而在紫外光辐射下硫醇被矿化并产生硫酸盐与碳酸盐。

     

    Abstract:  Layered K1-2xMxTiNbO5(M = Mn, Ni) was prepared by ion-exchange of KTiNbO5 obtained by the solidstate method with Mn2+ and Ni2+. The crystal structure and optical property of the as-prepared K1-2xMxTiNbO5 were studied by using powder X-ray diffraction and ultraviolet (UV)-visible light diffuse reflection spectroscopy. The adsorption feature and photocatalytic oxidation activity of dimethyl sulfide (DMS) and ethyl mercaptan (EM) over the as-prepared K1-2xMxTiNbO5 were evaluated using infrared spectroscopy. K1-2xMxTiNbO5 showed a higher interval between sheets and a stronger absorbance to visible light than KTiNbO5. After ion-exchange with Mn2+ and Ni2+, the bandgap energy of KTiNbO5 was shifted from 3.35eV to 2.97eV and 2.45eV, respectively, whereas the weak interaction between K1-2xMxTiNbO5 and DMS/EM was little affected by the exchanged cation. The photocatalytic oxidation activity of K1-2xMxTiNbO5 for DMS or EM depended on the special cation. K1-2xMnxTiNbO5 emerged a photocatalytic activity only under ultra-light irradiation, which converted DMS to sulfoxide and sulfone, and EM to sulfonic acid. However, K1-2xNixTiNbO5 emerged the photocatalytic activity under visible light besides under ultra-light irradiation; EM was converted to sulfonic acid by visible irradiation, but to sulfate and carbonate by UV radiation.

     

/

返回文章
返回